Fused Cast AZS 41 Brick

  • Price:

    Negotiable

  • minimum:

  • Total supply:

  • Delivery term:

    The date of payment from buyers deliver within days

  • seat:

    Henan

  • Validity to:

    Long-term effective

  • Last update:

    2020-02-29 13:58

  • Browse the number:

    487

Send an inquiries

Company Profile

Henan Caihui Kiln Material Co., Ltd

By certification [File Integrity]

Contact:caihui(Mr.)  

Email:

Telephone:

Phone:

Area:Henan

Address:Henan

Website:http://www.ch-refractory.com/ http://caihui.cndpmotors.com/

Product details

Product overview

Fused cast AZS 41 brick is the most excellent product in fused cast AZS series, it has the best corrosion resistibility to the molten glass, the glass phase exudation temperature is extremely high, and the pollution to the molten glass is extremely low. Therefore, it is usually recommended to be used in quick wear positions of glass kilns to balance the life of kiln, such as sidewall of the furnace hot point, doghouse corner, throat, weir block, Bubble block, etc and the furnace that require very high corrosion resistibility, like the whole electric furnace.


Character

Best corrosion resistance, very high glass exudation temperature, suitable for the important position of furnace to balance the furnace life. Such as doghouse corner, throat, weir block, bubble block and the whole electric furnace.


Casting methods

Casting Type

Name

Density

Application position

ZWS

Ending cast

≥ 3.85

sidewall

WS

Void free cast

≥ 3.9

sidewall, throat, doghouse corner, weir, bubble block, thermercouple block, etc


Specification

Chemical Composition

Item


Unit

AZS 41

Al2O3


%

Residue

ZrO2


40.0-44.0

SiO2

13

Na2O

1.3

(CaO+MgO+K2O+Fe2O3+TiO2+Na2O)

2.0

(Fe2O3+TiO2 )

0.3

Physical properties

True specific gravity

g/cm3

3.95

Apparent porosity

%

1.0

Melting glass erosion resisiting speed at static state(normal soda-lime glass, 1500℃*36h)

mm/24h

1.3

Temprerature of glass leaching

1400

Bubble separation ratio (normal soda-lime glass, 1300℃*10h)

%

1.0

Exudation (Volume %) (1500℃*4h)


%

3.0

Thermal expansion ratio(1000℃)


%

provide the actual test data

Bulk density Min. >

PT,QX

g/cm3

3.55

ZWS

g/cm3

3.85

WS

g/cm3

3.9

Note: Suitable to the single blocks over than 50 kg.


Thermal expansion curve:


Application

Container glass furnace  Whole Electric furnace


Production line of fused cast AZS refractory: